Grade | PSD/μm | Chemical/% | Test Frequency | 106 Ring 26.9*14.5*11.0mm |
Remark | |
D50 | C | O | Permeability (μi) | |||
T8L | 3.0-6.0 | ≤0.15 | ≤0.60 | 10kHz | ≥55 | |
T8L-I | 6.0-10.0 | ≤0.15 | ≤0.60 | 10kHz | ≥75 | |
T8S | 4.0-6.0 | ≤0.15 | ≤0.60 | 10kHz | 23-28 | |
T2L | 4.0-6.0 | ≤1.50 | ≤1.00 | — | — - |
|
T2A | 3.8-6.0 | ≤1.50 | ≤1.50 | 200KHz | 8.0-13.0 | |
T8A3(201) | 3.8-7.0 | ≤0.40 | ≤0.90 | 200kHz | ≥19 | 1g磁环 10.8*8.0*3.3mm |
T8A5(201) | 5.0-10.0 | ≤0.40 | ≤1.00 | 200kHz | ≥22 | 1g磁环 10.8*8.0*3.3mm |
T8SK | 4.0-7.0 | ≤0.30 | ≤1.00 | 100kHz | 21.0-26.0 | coating |
T8SK-B | 5.5-8.5 | ≤0.30 | ≤1.00 | 100kHz | 22.0-27.0 | coating |
T8A3 | 3-6 | ≤0.20 | ≤0.80 | 100kHz | 25.0-29.0 | coating |
T8A3-6JY | 5.0-8.0 | ≤0.20 | ≤0.80 | 100kHz | 26.0-30.0 | coating |
T8A5 | 3-6 | ≤0.30 | ≤1.00 | 200kHz | 23.0-29.0 | coating |
T6A | 1.2-2.2 | ≤1.80 | ≤1.80 | 25MHz | 8.0-11.0 | |
FeSiCr(-500) | 9.0-16.0 | <0.20 | <0.70 | 200kHZ | ≥27 | coating |
FeSiCr(-325) | 16.0-20.0 | <0.20 | <0.70 | 200kHZ | 30-34 | coating |
H8 | - | - | - | 200kHz | 25 | High temperature resistance |
The Global PM Database (GPMD) has been enhanced to include examples of PM microstructures, to assist PM parts ma
Metal soft magnetic powder core isproduced by powder metallurgy which based on metal soft magnetic and then coate
Yuelong GmbH, as the branch company of Jiangxi Yeuan Superfine Metal Co ,Ltd, will attend in the Euro PM 2017 C